The 15th International Symposium on Superalloys (Superalloys 2024) highlights technologies for lifecycle improvement of superalloys. In addition to the traditional focus areas of alloy development, processing, mechanical behavior, coatings, and environmental effects, this volume includes contributions from academia, supply chain, and product-user members of the superalloy community that highlight technologies that contribute to improving manufacturability, affordability, life prediction, and performance of superalloys.
Note biographique
Jonathan Cormier
ISAE-ENSMA
Ian Edmonds
Rolls Royce
Stephane Forsik
Carpenter Technology
Paraskevas Kontis
Norwegian University of Science and Technology
Corey O'Connell
Special Metals
Timothy Smith
NASA Glenn Research Center
Akane Suzuki
GE Global Research
Sammy Tin
Illinois Institute of Technology
Jian Zhang
Institute of Metals Research
Table des matières
Sustainability and Lifecycle Management of Nickel Superalloy Gas Turbine Components.- Microstructure Informatics of Polycrystalline Ni-base Superalloys Using Computer Vision Techniques to Understand Properties and Performance.- Optimizing Local Phase Transformation in Ni-based Superalloys Utilizing Thermodynamically Driven Design Framework and Multiscale Characterization.
Détails
Code EAN : | 9783031639364 |
Editeur : | Springer Nature Switzerland-Springer Nature Switzerland-Springer International Publishing |
Date de publication : | 21-08-2024 |
Format : | Relié |
Langue(s) : | anglais |
Hauteur : | 285 mm |
Largeur : | 215 mm |
Epaisseur : | 50 mm |
Poids : | 3297 gr |
Stock : | Impression à la demande (POD) |
Nombre de pages : | 1140 |
Mots clés : | Alloy development; Coatings on metals; Environmental effects of metal extraction; Mechanical behavior of Metal Alloys; conference proceedings; superalloys |